تآكل واجهات LED الساحلية
تآكل واجهات LED الساحلية
المعادن المختلفة والموصلات وحدود رذاذ الملح.
الآلية
Galvanic corrosion requires dissimilar metals, electrical contact and an electrolyte [S2]. Review housing, bracket, fastener, connector and substrate as one material stack.
مثال كمي
Illustrative screen: 100 interfaces with 300mm² cathodic area and 10mm² coating damage each produce a 30:1 exposed-area ratio. This identifies inspection priority; it is not a corrosion-rate prediction.
معايير الاعتماد
- Salt-mist hours are comparative, not a universal service-life conversion [S1].
- Repair field-drilled coating damage.
- Resolve corrosion isolation versus protective bonding.
- Technical reviewer: 待确认.
Sources
Author: LikeLight Tom, Operations. Evidence reviewed August 22, 2026.